Ultimate Tensile Strength
40 MPa 6 ksi -
Heat Deflection Temperature
60 °C 140 °F -
Elongation At Break
100 % -
Impact Strength (Notched)
15 J/m 0.28 ft-lb/in -
Tensile Modulus
1700 MPa 247 ksi - ABS, PMMA, POM
-
Ultimate Tensile Strength
35 MPa 5 ksi -
Heat Deflection Temperature
120 °C 248 °F -
Elongation At Break
100 % -
Impact Strength (Notched)
75 J/m 1.41 ft-lb/in -
Tensile Modulus
900 MPa 131 ksi - ABS, High-Performance (PEEK, PEI, PSU, PSSU), Polyamides / Nylons, Polycarbonate, Polypropylene, POM
-
Ultimate Tensile Strength
42 MPa 6 ksi -
Heat Deflection Temperature
53 °C 127.4 °F -
Elongation At Break
120 % -
Impact Strength (Notched)
50 J/m 0.94 ft-lb/in -
Tensile Modulus
1500 MPa 218 ksi - PMMA, Polycarbonate, Polypropylene, POM
-
Ultimate Tensile Strength
30 MPa 4 ksi -
Heat Deflection Temperature
45 °C 113 °F -
Elongation At Break
30 % -
Impact Strength (Notched)
30 J/m 0.56 ft-lb/in -
Tensile Modulus
1400 MPa 203 ksi - ABS, POM