Durometer (Shore A Hardness)
35 A -
Glass Transition Temperature
10 °C 50 °F -
Elongation At Break
350 % -
Tear Strength
10 kN/m 57.1 lbf/in -
Bayshore Resilience
20 % - SEBS TPE